Submit manuscript...
Journal of
eISSN: 2373-4345

Dental Health, Oral Disorders & Therapy

Case Report Volume 13 Issue 1

Success tips for renewing fractured ceramic veneer on central insicor

Yosra Farhat, Imen Kalghoum, Ines Azzouzi, Zohra Nouira, Belhssen Harzallah, Mounir Cherif, Dalenda Hadyaoui

Received: October 01, 2021 | Published: January 28, 2022

Citation: Farhat Y, Kalghoum I, Azzouzi I, et al. Success tips for renewing fractured ceramic veneer on central insicor. J Dent Health Oral Disord Ther. 2022;13(1):4-7. DOI: 10.15406/jdhodt.2022.13.00562

Download PDF

Abstract

This clinical report describes how to achieve a successful rebonding of a debonded porcelain veneer successfully using several procedures such as grinding enamel to eliminate the remaining adhesive from the first bonding and ultrasonic treatment of the veneer’s surface. Care is given the bonding protocol in order to optimize the durability of the interface. 

Keywords: Incisor, veneer, fracture, Rebonding, surface preparation, etching

Creative Commons Attribution License

©2022 Farhat, et al. This is an open access article distributed under the terms of the, which permits unrestricted use, distribution, and build upon your work non-commercially.